We can manufacture Graphene (rGO) in the form of a dispersion in various solvents, as well as in the form of a film with a thickness of 10 nm to 1 mm, paper or a powder according to your order. Place your order in this section and we will contact you to discuss the details.
Elemental composition of rGO (according to elemental analysis and XPS data):
C: 93.0 ± 0.7 ат.%
O: 6.0 ± 0.7 ат.%
S, N: < 0.5 ат.%
other impurities: < 0.5 ат.%
Functional composition of rGO (according to XPS data):
C(sp2): 93.2-94.9 at.%
C-OH & C-O-C: 3.3-4.7 at.%
C=O: 0.7-0.9 at.%
COOH: 1.1-1.2 at.%
C/O ratio (according to XPS data): 14.7-19.6